因此提高低氟烧结矿粘结相的熔点及结晶能力是降低微气孔率、提高强度的根本途径。
The basic way to decrease the pore number and improve the strength of the sinter with low fluorine is increasing the melting point and crystallization capacity of the binding phase.
结果表明; 随着烧结温度的升高,开口气孔率降低,断裂强度升高。
Results show that the open porosities are decreased and fracture strength is increased with the increase of the sintering temperatures.
随烧结温度的升高,材料的显气孔率降低,而体积密度、硬度和抗压强度均增加。
With the increase of sintering temperature, the apparent porosity of sample decreases, while bulk density, hardness and compressive strength increased.