湿接缝:指预应力混凝土梁体分块预制,悬臂拚装成大跨度连续梁,梁体间采用现浇混凝土把梁块连成整体的接缝。
Carries on the finite element analysis to the continuous beam,which uses different material in the wet joint,like high strength steel fiber reinforced concrete (HSFC) and common concrete.
对采用高强钢纤维混凝土为湿接缝材料与采用普通混凝土材料两跨连续梁进行有限元分析。
参考来源 - 先简支后连续梁桥湿接缝处纤维混凝土韧性试验研究It is suggested that structural reinforcement ratio of junction of wet-joint should be no less than 0.3%.
建议在工程应用中,湿接缝接头宜设计配筋率不少于0.3%的构造钢筋。