与此类似,渗碳层厚度越大,特别是对于渗碳层厚度不一的渗碳用钢,淬火时更易产生翘曲。
Sim? ilarly, an increase in case depth, particularly uneven case depth in case hardening steels, increases warpage on quenching.
当这种钢冷却时,就像图2.1的z - z线所示,除了初步的或预共析状态用渗碳体取代铁素体外,其余类似亚共析钢的情况。
When such steel cools, as shown in zz 'of Fig. 2.1 the process is similar to the hypo-eutectoid case, except that the primary or pro-eutectoid phase is now cementite instead of ferrite.