运用XRD、SEM以及强度实验等方法,研究了由石灰石、矿渣、石膏和少量熟料组成的石灰石基水泥的适宜配比和水化机理。
XRD, SEM, and strength test, were employed to investigate the appropriate ratio and hydration mechanism of limestone-based cement consisted of limestone, stag, gypsum and a small amount of clinker.
利用这些矿物材料和白水泥按照不同的配比制成多种板状矿物复合材料样品。
A number of samples of plank form mineral composite materials have been made from these mineral materials and white cement in different proportions.
该文结合工程实例介绍水泥稳定碎石的配比设计和施工工艺。
In the combination with the project example the paper introduces the mixture ratio design and construction process of cement stable broken stone.