通过分析光纤的过氧基缺陷,用氘气对成品低水峰光纤进行处理,以降低光纤的氢敏感性。
The low water peak fiber is treated by deuterium in order to reduce the fiber's hydrogen sensitivity based on the analysis of peroxide defects in fiber.
本文研究了铁中氢与辐照缺陷的相互作用。
The interaction between hydrogen and irradiated defects in iron was studied.
通过对产生锡汗缺陷的锡青铜铸件的显微组织和实际生产过程分析讨论了锡汗产生的原因,并探讨了较为经济实用的氧化去氢法消除锡汗的有效性。
Through analyzing the actual producing process and microstructure of the Sn-bronze castings with thedefect of stannic sweat, the cause resulting in the defect in the castings has been discussed.