木粉的碱化处理使复合材料的弯曲强度和弯曲模量分别下降20。
Alkaline treatment of wood flour makes flexural strength and flexural modulus of the composite decrease by 20.
以甲苯二异氰酸酯(TDI)为偶联剂将正辛醇接枝到杉木粉表面,同时考察处理前后杉木粉填充PP复合材料的力学性能。
Octanol was grafted onto fir powder using TDI as coupling agent, then its application in PP composite materials was investigated.
用硅烷偶联剂A - 171和天然橡胶胶乳(MGL - 30)改性碱处理后的橡胶木粉。
The alkali treated rubber wood-flour was modified by silane coupling agent A-171 and MMA grafted natural rubber MGL-30.