室温下固化,速度快,有利于提高产量。
Room temperature curing, high speed, help increase production.
常规室温下固化聚酯的经验法则是:直线每一英尺的收缩量为1/32英寸(当加强玻纤重量比为25%时)。
A general rule of thumb for conventional room-temperature cured polyesters is 1/32 inch of shrinkage per linear foot when reinforced with 25 weight percent glass content.
采用此方法增韧的环氧树脂,贮存稳定性好,在加热及室温条件下固化,均能获得较高的剪切强度和T -剥离强度。
The epoxy resin toughened by the above copolymer has excellent storage stability and, after cured by heating or at room temperature, it has higher shear strength and T-peeling strength.