在感应淬火中,通过改变加热时间、加热功率和冷却速度可以改变淬硬层深度和硬度梯度。
The hardening case depth and hardness curve can be changed by adjusting heating time, heating power and cooling speed during induction hardening.
随着提高加热温度和延长保温时间,“上坡扩散”的富磷层深度和浓度将不断增加。
With increase of heating temperature and duration of heating time, the depth and concentration of phosphorous-enriched layer in uphill diffusion increases continuously.
结果表明,两种弹簧钢的脱碳深度随提高加热温度和增加加热时间增大。
The result shows that the decarburization depth increases with the increase in temperature and holding time for the two steels.