论文
1.Preparation of hollow carbon nanospheres via explosive detonation .Materials Letters 63(2009)58-60 (SCI收录)
2.Preparation and mechanism of nanometer Al5N6 via shock wave plasma technique. Materals Recssearch Bulletin 44(2009) 198-201 (SCI收录)
3.Preparation of Nano-sized silver Powder via Active Template Process,THE CHINESE JOURNAL OF NONFERROUS METALS,2006,(6)(SCI)
4.The Influence of Particle Size of RDX on the Shock Sensitivities of RDX/F2641,5th International Symposium on Test and Measurement,2003,(Volume1) (EI)
5.Study on The attenuating Model of Detonation Shock wave in the PMMA, THEORY AND PRACTICE OF ENERGETIC MATERIALS 2001.10 (ISTP)
6.C/ZrO2复合纳米粉体的快速制备及其机理研究.高压物理学报.2008,22(2)131-136(Ei收录)
7.用爆燃法制备纳米氧化锆及其机理研究.材料研究学报.2008,22(5),550-554(Ei收录)
8.A15O6N纳米粉体的制备与表征.硅酸盐学报。2008,36(5),580-583(Ei收录)
9.活性模板法制备纳米镍粉体. 稀有金属材料与工程,2005,5(SCI收录,Ei收录)纳米α-Al2O3对HMX撞击感度的影响. 含能材料,2005,1(EI收录)
10.纳米Al2O3对HMX临界起爆压力的影响.测试技术学报2005,2(EI收录)
11.纳米Al2O3制备及其对HMX热感度的影响,应用基础与工程科学学报,2005,第4期.396~399(EI收录)
12.王作山,刘玉存,张景林,张包民.约束条件及装药直径对HMX/F2641传爆药爆压影响的实验研究,爆炸与冲击,2003,第3期,248~252 (EI收录)
专利
1、CN200310,114455.8 无团聚纳米α—Al2O3粉体的制备方法”发明专利,已授权
2、一种珊瑚状纳米α-Al2O3的快速制备方法,200810,023523.2