对微细高速钢麻花钻破坏断口进行了显微观察和测量,根据微小孔钻削实验结果,分析了造成钻头折断的原因和影响其使用寿命的因素。
The fault plane of micro-drill is measured with microscope. According to the result of test, the main elements of destroying drill is investigated.