阐述了各工艺步骤的配方及操作条件。过渡层采用高堆积碱铜,工作层为快速刷镀镍。
Formula and operating conditions of the procedures were described, high-packed alkaline copper deposit was adopted to act as interlayer and fast nickel brush deposit as working layer.