如超过最大重涂间隔,须磨粗表面,以确保漆膜间的附着力。
If maximum recoat interval is exceeded, roughen the film surface to ensure the adhesion between layers.
如超过最大重涂间隔,须磨粗表面,以确保漆膜间的附着力。
If maximum recoat is exceed, roughening of the surface is necessary to ensure intercoat adhesion.
目前,国内管道混凝土配重涂敷厂的生产装备基本为国外进口。
At present, the domestic production lines for concrete weight coating of submarine pipeline are basically imported.
重涂时间的间隔,由施工时的温度和涂膜固化的程度(以手触不粘)来确定。
The interval of the coating time is determined by the temperature at the time of construction and the degree of curing of the film (by hand).
适用范围广,可在室温和潮湿的环境中使用,并且对旧基材也有良好的重涂性。
Wide scope of application, can be at room temperature and humid environment in use, and the old substrate also has good recoatability.
可按照使用目的或区域修改漆膜厚度,但这会相应改变涂布率、干燥时间和重涂间隔。
May be specified in another film thickness than indicated depending on purpose of use and area. This will alter spreading rate, drying time and recoat interval.
对于附着力来说,无最大重涂间隔,但具体情况要视漆膜暴露于污染环境及加工中受损坏的程度而定。
No maximum recoat interval for adhesion, but dictated by gradual breakdown and damage during exposure and fabrication.
说明:混凝土配重涂层系统由水泥、水、骨料(按照具体的密度要求使用重骨料或轻骨料)和加固材料组成。
Desciption: Weight coating system composed of cement, water, aggregates, heavy or light depending on the required density and reinforcement.
说明:混凝土配重涂层系统由水泥、水、骨料(按照具体的密度要求使用重骨料或轻骨料)和加固材料组成。
Desciption: Weight coating system composed of cement, water, aggregates, heavy or light depending on the required density and reinforcement.
应用推荐