• 单板厚度干缩平均为6.8%,高于网带传送对流干燥单板3.3%; 纹于缩率4.8%,低于对流干燥的单板7.9%。

    The average thickness shrinkge rate (6. 5%) is higher than that of convection drying (3.3%) and cross-grain shrinkge rate (4.8%) is lower than that of convection drying 7. 9 %.