实验测得漂白后交联型材料的二阶倍频信号衰减了28%,而侧链型材料则衰减了75%。
After experimental bleaching a second order frequency-doubling signal of the cross-linked material has bee attenuated for 28%, but the side chain materia attenuated up to 75%.
实验测得漂白后交联型材料的二阶倍频信号衰减了28%,而侧链型材料则衰减了75%。
After experimental bleaching a second order frequency-doubling signal of the cross-linked material has bee attenuated for 28%, but the side chain materia attenuated up to 75%.