透射电镜观察表明,焊接接头各微区的显微硬度变化主要与时效强化相的析出行为有关。
TEM observation revealed that the changes in micro-hardness of micro-areas across the weld are mainly related with the precipitate evolution during the aging process.
结果表明,镍基单晶基体相和强化相均表现出明显的率相关性。
The effects of strain rate on the matrix and precipitate phases of Ni-base superalloy have been analyzed using the theory.
讨论了弥散强化铜合金强化相的选择原则,以及此合金的应用前景。
Selected principles of strengthening phase of dispersion strengthening Cu alloy and its application prospect were discussed.
对所有患者均进行双螺旋CT扫描,分别获取血管相和肝脏最大强化相影像。
Helical CT scan images were obtained in the vascular phase and the maximal hepatic enhancement phase.
在相同的体积分数下,随着涂层中弥散强化相尺寸的减小,涂层的耐磨性提高。
With the same additive volume, the abrasive resistance of the coating increases as the size of the dispersion strengthening phase decreases.
同时开裂倾向还受激光工艺参数、涂层合金粉的配比以及强化相的形状、大小等因素的影响。
At the same time, the cracking trend is affected by the laser cladding process parameters, the alloy powders content, and the shape and size of the reinforced phases.
结果表明,该缺陷与强化相析出有关,金相与电镜观察证明,该区域是析出质点富集区经氧化形成的。
The metalurgraphic and electron microscopic inspection found that the black spot defects are formed by the oxidation of particle enriched zone.
这两种相都能阻碍位错运动,对合金起到很好的强化作用。
All of the two phases can impede dislocation movement, also play a very important role for strengthening the alloys.
大众文化是同传统的精英文化相区别的,其娱乐、消闲、商业性的功能大大强化,而认识教育和审美的功能相对弱化。
The culture of masses is different from that of traditional elite, and its function of entertainment, pastime and commerce is greatly strengthened.
方法观察完整时相,分析初始强化形式及与二维图像、CDFI的关系。
Methods The whole manifestation phases were observed to analyze the early enhancement forms and the relationship of the images with B-mode image and CDFI.
方法:观察完整时相,确定时间窗。分析初始强化形式以及该形式与二维图像、CDFI的关系。
Methods Whole phase manifestation was observed to determine the time-window and to analyse the early enhancement forms and the relationship between enhanced image and B-mode image and CDFI.
认为固溶强化和第二相强化是加入合金元素强化镁合金的主要方式。
It is thought that solution strengthening and second phase strengthening are two main ways for improving mechanical properties of magnesium alloy.
这种粒状组织,与针状铁相相比,对合金性能的影响要小得多,甚至可以起到强化组织的作用。
This kind of granular structure is less harmful to the properties of the alloy than the needle like iron phase, and even can be functional to strengthen structure.
两汉以降,相权的弱化与君权的强化是一个总体的历史趋势。
Since the two han Dynasty, the increasingly weakening premier power and enhancing counterpart had been a general historical trend.
复合材料常温和高温的拉伸断裂模式与基体相的形变强化特性有关。
The rupture mode of the composite at room and elevated temperature depends upon the work-hardening characteristics of the nickel alloy matrix.
为了使用者共同之利益,本国际标准已与ISO 14001: 1996相调和,以强化两个标准之兼容性。
This International standard has been aligned with ISO 14001:1996 in order to enhance the compatibility of the two standards for the benefit of the user community.
利用等离子体增强化学气相沉积(PECVD)工艺,在不同射频功率,不同反应气压条件下制备了氮化硅薄膜。
SiN thin films are deposited by plasma enhanced chemical vapor deposition (PECVD) under various power and pressure conditions.
采用甚高频等离子体增强化学气相沉积技术制备了不同衬底温度的微晶硅薄膜。
A series of microcrystalline silicon thin films were fabricated by very high frequency plasma-enhanced chemical vapor deposition at different substrate temperatures (T_s).
传统等离子体增强化学气相沉积(PECVD)技术,工艺成熟,制备的薄膜质量高,较适合大规模工业化生产。
For the high technical maturity and the high deposition quality, traditional plasma enhanced chemical vapour deposition (PECVD) technology was wide applied in the large-scale industrial production.
从基体组织和沉淀相质点等方面分析了时效强化铝合金机械性能的变化规律。
From base structures and precipitated phase particles and other aspects, this paper analyses the changing laws of age-hardening aluminium alloys 'mechanical properties.
采用甚高频等离子体增强化学气相沉积技术制备了不同衬底温度的微晶硅薄膜。
Microcrystalline silicon thin films prepared at different deposition parameters using very high frequency plasma enhanced chemical vapor deposition (VHF-PECVD).
采用射频等离子体增强化学气相沉积法(RF - PECVD)在钢衬底上沉积氮化硅薄膜。
Silicon nitride thin films were prepared onto steel substrates by radio-frequency plasma enhanced chemical vapor deposition (RF-PECVD) technique.
在较佳具体实施例中,该共沉积作用系以等离子体强化化学气相沉积法进行。
In a preferred embodiment, the codeposition is carried out by plasma enhanced chemical vapor deposition.
以硅烷和氧化二氮作为反应气体,采用等离子体增强化学气相沉积(PECVD)技术,不使用掺杂,在单晶硅衬底上制备了用于平面光波导的二氧化硅薄膜。
Without doping, plasma enhanced chemical vapor deposition (PECVD) of silica films on si substrates with gas mixtures of SiH_4 and N_2O is considered.
结论结核瘤动态增强CT扫描在强化值、时间一密度曲线及强化形态均有一定特征,可与周围型肺癌及炎性肿块相鉴别。
Conclusion: Tuberculoma can be differentiated from peripheral pulmonary carcinoma or inflammatory mass by the characteristic of maximum enhanced ct value, enhanced pattern and time-attenuation curves.
在反应器中固液两相进行高效的混合,强化反应过程的传热和传质效率。
A solid phase and a liquid phase are efficiently mixed in the reactor in order to enhance the heat and mass transfer efficiency during the reaction.
依此较好地解释了相分析结果与电磁性能间的不一致,并提出了强化2223相形成的措施。
Thus, the irregularity between the results of phase analysis and electric, magnetic properties can be explained, and the measures of consolidating 2223 phase can be determined.
本文将三相流强化传热技术应用于重力热管,构建了三相流闭式重力热管系统。
In this paper, the three-phase flow heat transfer enhancement technique is applied to closed gravity heat pipe and a set of three-phase flow gravity heat pipe system is set up.
采用甚高频等离子体增强化学气相沉积技术成功地制备了不同硅烷浓度和辉光功率条件下的微晶硅电池。
Microcrystalline silicon solar cells with the variation of silane concentration (SC) and discharge power were fabricated by very high frequency plasma-enhanced chemical vapor deposition.
采用甚高频等离子体增强化学气相沉积技术成功地制备了不同硅烷浓度和辉光功率条件下的微晶硅电池。
Microcrystalline silicon solar cells with the variation of silane concentration (SC) and discharge power were fabricated by very high frequency plasma-enhanced chemical vapor deposition.