CBN is an ideal tool material for finish and semi_finish turning powder superalloy. It not only ensures the high machining accuracy, but also can obtain longer tool life.
对精车和半精车而言,CBN是车削粉末高温合金的一种理想刀具材料,它不仅可保证高的加工精度,而且可获得长的刀具寿命。
The research is useful in selecting the tool geometry, coolant and cutting parameters in machining this kind of superalloy.
研究工作对该材料加工过程中的切削用量、冷却液和刀具几何参数等的选择具有指导和参考意义。
The numerical result provides the theoretical reliance for optimization of the laser cladding parameters on K418 superalloy.
计算结果为优化K418高温合金激光熔覆工艺参数提供了理论依据。
The products by ESR include 243 designations of steel and superalloy.
产品包括优质合金钢与超级合金243个牌号。
Fretting wear behavior of K417 nickel base superalloy was investigated.
研究了K417镍基高温合金的微动磨损行为。
The aluminized coating on K438 superalloy was prepared by pack cementation.
采用固体粉末包埋渗铝法,在K438高温合金表面制备渗铝涂层。
The results show that single crystal superalloy DD6 has good creep properties.
结果表明,DD6合金的蠕变性能良好,并具有蠕变各向异性;
An experimental study on the fatigue crack growth of GH4169 superalloy has been carried out.
本研究中对GH4169高温合金的疲劳裂纹扩展性能进行了试验研究。
The casting process of fine grain K418 superalloy blades has been investigated in this paper.
研究了K418高温合金细晶叶片铸造工艺。
In this paper the role and distribution of La in the Co-base superalloy GH188 are investigated.
本文研究了镧在钴基超合金GH188中的作用及其分配。
A new method to free forge the blank of case of an aircraft made of superalloy has been studied.
本文研究了一种自由锻造耐热合金机匣毛坯的新方法。
The most active research has been applied to aluminium, iron, copper based alloys and superalloy.
其中以铝基合金、铁基合金、高温合金及铜合金方面的研究最为活跃。
The products of electroslag remelting steel include 243 designations of alloy steel and superalloy.
产品包括优质合金钢与超级合金243个牌号。
The results are beneficial to grinding this new type superalloy with high efficiency and high precision.
旨在为寻求优化的高效、高精度磨削加工工艺提供理论及试验依据。
The anisotropy of compression creep strength in a nickel-base single crystal superalloy was investigated.
研究了镍基单晶高温合金压缩蠕变强度的各向异性。
Addition of Hf to a superalloy is one of the effective approaches to improve its mid-temperature properties.
添加铪是改善合金中温性能的有效途径之一。
The second moment creep time of DZ4 superalloy rapidly decreases with the increasing of temperature and stress.
随着温度的升高和应力的增加,DZ 4合金蠕变第二阶段的时间迅速减少。
The work in this paper can provide useful information for isothermal forging process of P/M superalloy turbine disk.
本文的研究结果为实现粉末高温合金盘件超塑性等温锻造奠定了基础。
The effect of withdrawing rate on the solidification microstructure of a single crystal superalloy DD6 was investigated.
研究了不同的抽拉速率对第二代单晶高温合金dd 6凝固组织的影响。
The existing points and the research direction in future for powder metallurgical superalloy are presented in this paper.
文中提出粉末冶金高温合金存在的问题及今后的研究方向。
The effects of electric field treatment on the microstructure and deformation behavior of GH4199 superalloy were studied.
将电场处理技术应用于GH4199合金,研究电场对该合金组织和变形行为的影响。
The results can meet the requirements about qualitative analysis and semi-quantitative analysis of tungsten in superalloy.
研究结果可用于高温合金中钨元素的定性和半定量分析及材料牌号鉴别。
The effects of strain rate on the matrix and precipitate phases of Ni-base superalloy have been analyzed using the theory.
结果表明,镍基单晶基体相和强化相均表现出明显的率相关性。
Low cycle fatigue (LCF) tests of a directionally solidified nickel base superalloy were conducted at elevated temperatures.
本文研究了一种定向凝固镍基高温合金的高温低周疲劳行为。
The effect of melt overheating treatment on the solidification segregation of M963 cast Ni-base superalloy has been studied.
研究了熔体过热处理对M963铸造镍基高温合金凝固偏析的影响。
This article studies a new type cobalt-base superalloy GH941 including its composition, structures and mechanical properties.
本文研究了新型钴基高温合金GH941的成分、组织及性能。
The aluminizing process by low press packing cementation(LPPC) on the surface of K17 superalloy was investigated in this paper.
研究了在高温合金K17表面上低压固体粉末包埋(LPPC)渗铝工艺。
Superalloy GH4169 has been used as the main object of study to discuss the grinding characteristics of nickel based superalloy.
以GH4169高温合金为主要研究对象,论述了高温合金的磨削特征。
Superalloy GH4169 has been used as the main object of study to discuss the grinding characteristics of nickel based superalloy.
以GH4169高温合金为主要研究对象,论述了高温合金的磨削特征。