• The results show that X80 pipeline steel obtains sorbite after quenching and tempering, gets pearlite by normalizing.

    结果表明:x80钢经调质处理后得到索氏体,正火得到珠光体。

    youdao

  • With the decrease of finishing rolling temperature, the grain size is refined apparently and the contents of sorbite is increased.

    随着终轧温度的降低,热轧材组织得到细化,索氏体含量提高。

    youdao

  • The results indicate that, with the increase of rolling times, the grain size becomes smaller, the content of sorbite multiplicates, and the yield strength improves.

    结果表明,随轧制道次的增加,晶粒尺寸逐渐减小,索氏体的含量不断增加,屈服强度逐渐提高。

    youdao

  • The results show that 82b wire rod brittle fracture is mainly caused by excessive inclusion, reticulate carbide, lower sorbite in the microstructure, and surface defect of wire rod.

    结果表明,82B钢盘条脆断的主要原因是夹杂物级别超标、组织中出现网状碳化物、索氏体含量偏低以及盘条表面缺陷等。

    youdao

  • The results indicated that the tempered sorbite was the optimum microstructure, the inhomogeneous distribution of micro hardness affected markedly the finish quality of the steel surface.

    结果表明:回火索氏体是最佳的组织形态;微观硬度的不均匀性显著影响钢的表面加工质量。

    youdao

  • The results indicated that the tempered sorbite was the optimum microstructure, the inhomogeneous distribution of micro hardness affected markedly the finish quality of the steel surface.

    结果表明:回火索氏体是最佳的组织形态;微观硬度的不均匀性显著影响钢的表面加工质量。

    youdao