The major reasons for terminal post corrosion of valve regulated lead-acid batteries are explained. Some sealing methods and influence factors are discussed.
论述了阀控密封铅蓄电池极柱腐蚀的原因。讨论了端极柱密封的方法和影响端极柱密封性能的主要因素。
In order to acquire a good hermetic seal between the diaphragm and the base plate, two sealing methods were used, namely, compound method and crystallite method.
研究了复合法和结晶法两种封接方式,使陶瓷基座与膜片达到良好的匹配封接。
In order to acquire a good hermetic seal between the diaphragm and the base plate, two sealing methods were used, namely, compound method and crystallite method.
研究了复合法和结晶法两种封接方式,使陶瓷基座与膜片达到良好的匹配封接。