There are a series of problems in batch production of plating chromium for lining inner bores of input tube in oil well pump such as parameter choice, clamp design, bath care and adjust.
油井抽油泵输入泵衬套内孔尺寸镀铬批量生产中存在着工艺参数准确选择、夹具合理设计、槽液维护和调整等一系列问题。
The inner anode and its choice for copper plating on stainless steel was emphatically introduced.
重点对不锈钢镀铜的内阳极及其选择作了介绍。
The corrosion resistance of deposits and covering power of the plating bath were tested respectively by neutral salt spray test and inner-pole method, and the hardness of deposits was also measured.
采用中性盐雾试验测定了镀层的耐蚀性,采用内孔法测定了镀液的覆盖能力,并测定了镀层的硬度。
It can also avoid pretermission of plating, burnout of zinc layer on weld beam and heat affected zone, and other limitations on the inner surface of fuel tank made of galvanized sheet.
从而避免了传统电镀锌板直接焊接成型油箱内表面漏镀、焊缝及热影响区锌层烧损等缺陷。
The device comprises a workpiece to be plated, a workpiece clamping sealing device, a plating pen special for inner bore brush plating, and a plating pen rotary actuator.
该装置包括待镀工件、工件装夹密封装置、内孔刷镀专用镀笔、镀笔转动装置。
A circular tube-like gap (S1) in which a plating liquid (17) flows is formed between the tubular electrode placed in the hollow section and an inner peripheral wall (14) of the hollow section.
圆管状间隙(S1)在放置在中空段内的管状电极与中空段的内周壁(14)之间形成,电镀液在该 间隙(S1)中流动。
A circular tube-like gap (S1) in which a plating liquid (17) flows is formed between the tubular electrode placed in the hollow section and an inner peripheral wall (14) of the hollow section.
圆管状间隙(S1)在放置在中空段内的管状电极与中空段的内周壁(14)之间形成,电镀液在该 间隙(S1)中流动。