• Steels having less than the eutectoid amount of carbon (less than 0.77%) are known as hypo-eutectoid steels.

    含碳量少于共析体(低于0.77%)的钢称为亚共析钢

    youdao

  • Steels shaving less than the eutectoid amount of carbon (less than 0.77%) are known as hypo-eutectoid steels.

    含碳量少于共析体(低于0.77%)的钢称为亚共析钢

    youdao

  • When such steel cools, as shown in zz 'of Fig. 2.1 the process is similar to the hypo-eutectoid case, except that the primary or pro-eutectoid phase is now cementite instead of ferrite.

    这种冷却时就像2.1z - z线除了初步共析状态用碳体取代铁素体外,其余类似亚共析钢情况

    youdao

  • When such steel cools, as shown in zz 'of Fig. 2.1 the process is similar to the hypo-eutectoid case, except that the primary or pro-eutectoid phase is now cementite instead of ferrite.

    这种冷却时就像2.1z - z线除了初步共析状态用碳体取代铁素体外,其余类似亚共析钢情况