• The main wear mechanisms are adhesion, diffusion and fatigue.

    磨损机理主要是粘结磨损、扩散磨损以及疲劳磨损。

    youdao

  • The experimental results on commercial pure titanium verify the obvious changes in the microstructure, hardness and wear resistance after laser solid diffusion treatment.

    对工业纯钛的初步试验结果表明,用激光进行固态扩散渗氧处理可以明显改变钛表层组织、硬度和耐磨性。

    youdao

  • The results of experiments showed that the Nb can raise the depth of diffusion zone, hardness, wear resistance, strength and toughness of the nitriding layer of the matrix steel.

    实验结果表明,铌能增加扩散层深度、硬度及耐磨性,提高渗层的强韧性。

    youdao

  • The results of experiments showed that the Nb can raise the depth of diffusion zone, hardness, wear resistance, strength and toughness of the nitriding layer of the matrix steel.

    实验结果表明,铌能增加扩散层深度、硬度及耐磨性,提高渗层的强韧性。