• The ingots of cast superalloy K4169 was refined with the addition of a trace of intermetallic compounds to the melt under conventional casting condition.

    采用一种新型中间合金复合细化剂,在常规生产工艺条件下对高温合金K4169铸件进行了晶粒细化。

    youdao

  • In this paper the effects of pouring temperature, mold temperature, inoculants, and section size on the microstructure and mechanical properties of casting nickel-base superalloy K24 were studied.

    本文研究了浇铸温度、铸型温度、孕育剂和截面尺寸对K 24镍基铸造高温合金的组织和性能的影响。

    youdao

  • This paper introduces the casting precipitation properties, their effects on the alloy microstructure and the methods to eliminate the precipitation of the Low-expansion superalloy GH909. and GH907.

    本文研究了低膨胀高温合金GH907、GH909铸态组织中偏析的性质,偏析对合金组织的影响,以及消除偏析的方法。

    youdao

  • In order to improve the inner quality of superalloy master ingots, a technology of vacuum electromagnetic casting was developed for the superalloy, I.

    为了提高高温合金母合金锭的内在质量,提出了在高温合金真空熔铸的凝固过程,施加电磁搅拌的真空电磁铸造技术。

    youdao

  • The casting process of fine grain K418 superalloy blades has been investigated in this paper.

    研究了K418高温合金细晶叶片铸造工艺。

    youdao

  • Effects of the casting technological factors on the size and uniformity of surface grains of turbine blade castings in ni based superalloy were studied by comparison of experimental results.

    对比研究了铸造工艺参数对镍基高温合金叶片表面晶粒度和晶粒均匀度的影响。

    youdao

  • Effects of the casting technological factors on the size and uniformity of surface grains of turbine blade castings in ni based superalloy were studied by comparison of experimental results.

    对比研究了铸造工艺参数对镍基高温合金叶片表面晶粒度和晶粒均匀度的影响。

    youdao