The applicability of this method to cast nickel-base superalloy K417 is assessed and suitable life predictive methods are suggested for cast superalloy K417.
对此方法应用于铸造镍基高温合金K417的适用性进行了分析,并提出了适用于铸造高温合金K417的寿命预测方祛。
The effect of melt overheating treatment on the solidification segregation of M963 cast Ni-base superalloy has been studied.
研究了熔体过热处理对M963铸造镍基高温合金凝固偏析的影响。
The tensile, creep and stress-rupture properties at high temperature of a cast nickel-base superalloy K46 without cobalt, as comparison with superalloy K412, were investigated.
研究了一种无钴镍基铸造 高温合金K46的高温拉伸、蠕变和持久性能,并与K412合金进行了比较。
The tensile, creep and stress-rupture properties at high temperature of a cast nickel-base superalloy K46 without cobalt, as comparison with superalloy K412, were investigated.
研究了一种无钴镍基铸造 高温合金K46的高温拉伸、蠕变和持久性能,并与K412合金进行了比较。