采用此方法增韧的环氧树脂,贮存稳定性好,在加热及室温条件下固化,均能获得较高的剪切强度和T -剥离强度。
The epoxy resin toughened by the above copolymer has excellent storage stability and, after cured by heating or at room temperature, it has higher shear strength and T-peeling strength.
通过使用本实验室设计的低温拉伸夹具,测定了纳米二氧化硅改性环氧树脂复合材料在室温和液氮(77K)环境下的拉伸强度、弹性模量和延伸率。
Measurement of tensile strength , modulus and strain of nanometer SiO2/epoxy composite materials was conducted using self-designed tensile testing jigs at room temperature and 77K.
通过使用本实验室设计的低温拉伸夹具,测定了纳米二氧化硅改性环氧树脂复合材料在室温和液氮(77K)环境下的拉伸强度、弹性模量和延伸率。
Measurement of tensile strength , modulus and strain of nanometer SiO2/epoxy composite materials was conducted using self-designed tensile testing jigs at room temperature and 77K.