由于防倒块厚度不大,焊缝截面尺寸较小,承载能力不强;
As a result of anti-block thickness was not weld cross-section of smaller sizes, and carrying capacity is not strong;
为焊缝截面形态的预测及焊接规范参数的设计提供了依据。
These models not only establish a basis for the forecasting of welding section form, but also furnish a basis in the designing of welding process parameters.
随焊接热输入和激光功率密度的增大,焊缝截面由钉形向近X形转变。
With increase of heat input and laser power density, the cross section of the weld transformed from nail shape to near X shape.
热处理前后焊缝截面显微硬度均自焊缝中心向热影响区逐渐降低,热影响区显微硬度低于母材。
The microhardness of the weld bead reduces from the center of joint to base metal before and after heat treatment, and the microhardness of HAZ is minimum.
分析了入射角改变对焊接件外观形貌、焊缝截面、焊缝板间连接宽度以及所承受的拉剪载荷的影响。
The transverse weld topography, the connect width between plates and tension and shear load were analyzed when the incident angle changed.
采用模拟时的焊接工艺参数进行钨极氩弧焊平板对接焊,测定焊接热循环曲线和焊缝截面尺寸,对模拟结果加以验证。
The welding thermal cycle and section dimensions of the welding seam were measured in the condition of the simulated welding process parameters for checking simulation results.
结果表明,随激光功率增大和焊接速度降低,复合焊与单一激光焊焊缝的横截面形貌均由钉形向近X形转变。
It showed that the weld cross section with both laser welding processes transformed from nail shape to near X shape with increase of laser power and decrease of welding speed.
对某在用市政钢箱梁桥的动力特性、焊缝缺陷、应力和变形、钢构件截面尺寸和锈蚀情况进行了检测,按规范要求验算了结构的整体稳定和局部稳定。
It was examined that the dynamic peculiarity, the welding line flaw, the size of steel member section and the rusty phenomenon of an existing municipal steel-box girder bridge.
箱形截面构件薄壁板与内隔板电渣焊接时,易产生壁板烧穿和焊缝未熔合现象。
The weld defects of incomplete fusion and burn through always occur when the electro-slag welding is used between the outside thin metal plate and the inner clapboard in a box-section member.
桥式起重机采用工字形截面作为主梁,使用多年后该结构形式的主梁上翼缘板和腹板连接的主焊缝及母材多处产生裂纹,甚至发生主梁断裂事故。
Cracks occurred in the main weld joining the web and upper wing panel of an overhead crane girder of I-section, some of which have expanded to the structure material and even led to girder fracture.
X65管线钢在焊接过程中,内侧焊缝金属出现横向和纵向沿熔合线方向的裂纹,横向裂纹贯穿焊缝金属横截面。
The longitudinal cracks along bond line and the transverse cracks which cut across the weld metal cross section inside weld metal were formed, while X65 pipe line steel was welding.
受厚板截面本身的几何形状所影响,箱形截面有焊缝一侧壁板与另一侧壁板残余应力分布及大小有明显的不同。
Affected by the geometry of box-section, the residual stress distribution of plate with welding passes is different from that of another plate.
结果表明:焊接接头横截面宏观结构特征表现为焊核区的“洋葱环”和热-机械影响区的塑性流线变形,洋葱环的环间距随着距焊缝中心距离的增大而减小;
The experiment result shows that the spacing of onion rings, which is the most prominent features of most friction stir welds, decreases with the distance of onion ring to centerline increasing .
在显微硬度测试中,在焊缝试样横截面上用锥形金刚石压入23或更多的点。
In the microhardness survey test, a pyramid-shaped diamond is impressed into 23 or more points across the face of a weld sample cross section.
随着搅拌头平移速度的增加,垂直于焊缝方向上的截面上,等效塑性应变减小,但是材料的流动速度会随之增加。
With the increase of the translation velocity of the pin, the flow of the material in friction stir welding becomes faster but the equivalent plastic strain decreases.
随着搅拌头平移速度的增加,垂直于焊缝方向上的截面上,等效塑性应变减小,但是材料的流动速度会随之增加。
With the increase of the translation velocity of the pin, the flow of the material in friction stir welding becomes faster but the equivalent plastic strain decreases.
应用推荐