激光扫描路径和扫描速度影响每层加工时间。
The laser scanning paths and scanning speed usually influence the machine time of each section.
随扫描速度增加,界面形态由平直向波浪形变化;
The fluctuation is enhanced with the increasing of scanning velocity.
喷嘴移动扫描速度对铜电铸层多孔结构有明显的影响。
The scanning speed of nozzle has a great effect on the pore structure of copper deposits.
不到1秒的快速扫描速度使这套系统能够满足生产线的需要。
With scan times of less than a second, the system is fast enough to be used on a production line.
激光扫描速度对相变硬化区和热影响区的大小有极大的影响。
Furthermore, the scanning speed has an important influence on the size of phase change region and thermally affected region.
扫描速度一定时,扫描路径的优化与否将直接影响加工时间。
If the scanning speed is not changed, the optimization of scanning paths will directly influence the machine time of each layer.
总结了数字示波器垂直偏转灵敏度和水平扫描速度的检定工作。
Verification works on vertical deflection sensitivity and horizontal sweep speed of digital oscilloscope are summarized.
理论分析表明,合适的电位扫描速度依赖于腐蚀体系的电化学参数。
A theoretical analysis shows the suitable rate for potential sweep depends on electrochemical parameters of corrosion system.
研完了表面状态、斑尺寸、率及扫描速度对硬化层特征及耐磨性的影响。
The influence of coating, spot size, power and scanning speed on hardening layer features and wear resistance were studied.
熔化层的横截面积与激光束扫描速度之间在一定条件下接近双曲线关系。
The relationship between the section area of the molten layer and the scanning speed of the laser beam is close to hyperbolic under certain conditions.
结果表明,电位扫描速度和电位阶跃频率对裂纹萌生与扩展有显著影响。
The results indicated that potential scan rate and step frequency played an essential role in the initiation and propagation of crack.
暗化程度和折射率改变随激光强度、扫描速度、扫描行间距变化而变化。
Darkening and refractive index change varied with laser intensity, scan speed and line interval.
结果表明,预处理、送粉量、激光的扫描速度是决定模具修复质量的关键。
The results show that repairing quality of the dies is affected by pretreatment, laser power scanning rates and powder feed rates.
有一件事我们没有注意到的是,加州似乎是扫描速度与今年的版本的产品。
One thing we did notice is that ca seems to be scanning faster with this year's version of the product.
借助磁通反馈环节控制磁化电流扫描速度,使得产生的感应电压接近常数。
With the help of the sweeping velocity of magnetizing current controlled by a flux feedback loop a nearly constant induced voltage is produced.
激光功率的增大、扫描速度的减少都会使硬化层深度和硬化层宽度得到增加。
The depths and widths of the hardened band rises with increase in laser power or decrease in laser scanning velocity.
超声所考虑的每秒25扫描速度的快速图像创建移动、 生活类似的图片。
The ultrasound creates a moving, life-like picture by taking rapid images with the speed of 25 scans per second.
研究了激光功率,频率,扫描速度等参数及加工程序对芯片加工质量的影响。
The effects of laser power, frequency, writing speed and procedures on the quality of the chip was evaluated.
在扫描速度恒定的条件下,得出各路径及声源对扫描线的误差分布函数图形。
The error curves of different paths and sources vs scanning line number mare obtained.
文中给出了选择电位扫描速度的简单方法,讨论了这种方法在酸洗缓蚀剂试验中的应用。
A simple method of selecting potential sweep rate is given in the paper. The application of this method in acid cleaning inhibitor is discussed.
同相轴长度一定的情况下,扫描速度相同时,同相轴起始道序号越小,检测snr越好。
In the condition that the length of the event and the scan velocities are fixed, the smaller the serial number of the start channel of the event is, the better the detection SNR is.
系统研究了激光功率、扫描速度、预热温度、铺粉厚度等工艺参数对成型试样质量的影响。
The effects of different process parameters such as laser power, scanning speed, preheat temperature, powder-bed depth on the sintered quality were studied systematically.
分析了主要工艺参数如:激光功率、扫描速度、送粉量以及Z轴增量对成型质量和形貌的影响。
The technics parameters, such as the laser power, scan velocity, powder feed rate and the Z axis increment, which influence quality and shape were analyzed in this article.
随激光扫描速度增大,试样中的马氏体和未溶碳化物的含量不断增加,残余奥氏体含量则连续下降。
The martensitic and undissolved carbide contents continuously increase as the laser scanning speed increases while the residual austenite decreases.
适当选择衬底温度、激光功率和扫描速度可望获得良好的结晶,它对SO I器件的制作是有意义的。
If we select substrate temperature, laser power and the scan speed properly, we can get good crystallization. It is useful to the fabrication of SOI devices.
结果表明:循环伏安曲线为矩形特征,炭黑电极表现出典型的电容行为,扫描速度与比电容基本无关;
It was showed that the rectangular CV curves and linear potential-time curves exhibited typical capacitive behavior of CB electrode.
试验表明:通过调节激光器的输出功率、光斑直径和扫描速度可以方便地控制熔化层深度和表面平整度。
The experimental result shows that the depth of hardened zone and smoothness of surface can be controlled conveniently by varying the power output beam diameter and scanning rate of laser light.
通过改变送粉激光熔覆过程中的扫描速度、送粉速率、基体预热温度等工艺参数,获得了单道激光熔覆层。
Single pass laser surface of the specimens using powder feeding method were obtained by varying the powder feeding rate and the preheating temperature of the substrate.
通过改变送粉激光熔覆过程中的扫描速度、送粉速率、基体预热温度等工艺参数,获得了单道激光熔覆层。
Single pass laser surface of the specimens using powder feeding method were obtained by varying the powder feeding rate and the preheating temperature of the substrate.