The improved external arc roll body is provided with a cooling groove; the cooling groove is uniformly distributed on the roll body.
改进后所述外弧辊辊身上设有冷却槽,冷却槽呈环形均布在辊身上。
Roll fracture often takes place in hot rolling section steel. The fracture position is mainly located at the roll caliber, roll neck and boundary between the roll neck and roll body.
热轧型钢过程中经常发生轧辊断裂现象,断裂部位主要在轧辊的孔型处、辊颈处及辊颈与辊身交界处。
The results showed that the higher internal stress and serious carbide network in the banded carbide in the inner roll body were the main causes of heavy back-up roll stationary cracking.
结果表明,辊身心部较高的内应力和在带状碳化物中存在严重的网状碳化物是造成大型支承辊置裂的主要原因。
The influences of cooling rate of the mould, pouring temperature, nodularity and chemical composition on hardness of roll body were described, and the measures for solve problems were proposed.
对铸型冷却速度、浇注温度、球化率和化学成分对辊身硬度的影响进行了论述,并提出了解决问题的措施。
In this article author puts emphasis upon the discussion about distribution regularity of roll flattening along the length of roll body and optimum roll-bending force, which is of certain value.
本文重点讨论轧辊弹性压扁沿辊身长度分布的规律及最佳弯辊力,有一定参考价值。
In this article author puts emphasis upon the discussion about distribution regularity of roll flattening along the length of roll body and optimum roll-bending force, which is of certain value.
本文重点讨论轧辊弹性压扁沿辊身长度分布的规律及最佳弯辊力,有一定参考价值。