This initial reaction or oxidation resists further chemical reaction on the metal surface.
初始的反应或氧化可以抵制材料表面再进行化学反应。
In the initial stage of production, the film surface will produce "crystal point or impurity."
在生产的初始阶段,薄膜表面会产生‘晶点’或杂质。
The results show that different initial value give inconsistent surface abundance of heavy element.
结果表明,不同初值得到不同的表面重元素丰度分布。
The surface microhardness had improved from 160HV0.05 of the initial sample to 335HV0.05 after CRPD.
样品表面的显微硬度值达到了335HV0.05,与基体相比表面硬度提高两倍左右。
The surface microhardness had improved from 160HV0.05 of the initial sample to 335HV0.05 after CRPD.
样品表面的显微硬度值达到了335HV0.05,与基体相比表面硬度提高两倍左右。