• 一样温度请求相同厚度时高温浸镀所需时刻

    Not the same temperature, request the same thickness, high dip required a long time.

    youdao

  • 结果表明,钢丝时走速过快不均匀导致扭转脆性断裂主要原因

    And quick wire movement during hot-dipping and inhomogeneous coating was identified as the main cause.

    youdao

  • 结果表明,钢丝时走速过快不均匀导致扭转脆性断裂主要原因

    And quick wire movement during hot-dipping and inhomogeneous coating was identified as the main cause.

    youdao