Long glass fiber (LGF) reinforced ABS composite was prepared by means of a new method.
采用悬浮浸渍拉挤成型法制备长玻纤增强ABS复合材料。
The LGF was dipped into suspending intermediate, dryed, molten to draw- extruded to be bar, pelleted and molded.
该方法采用中间体悬浮液浸渍玻璃纤维,烘干,熔融状态下拉挤成棒型,切粒,注射成型。
The LGF was dipped into suspending intermediate, dryed, molten to draw- extruded to be bar, pelleted and molded.
该方法采用中间体悬浮液浸渍玻璃纤维,烘干,熔融状态下拉挤成棒型,切粒,注射成型。