The pretreatment of silver concentrate with high arsenic, antimony and copper is followed by in-pulp electrolysis, the leaching rate of silver is over 95%.
富含砷、锑、铜的银精矿先经过预处理,再进行矿浆电解,银的浸出率达到95%以上。
The pretreatment of silver concentrate with high arsenic, antimony and copper is followed by in-pulp electrolysis, the leaching rate of silver is over 95%.
富含砷、锑、铜的银精矿先经过预处理,再进行矿浆电解,银的浸出率达到95%以上。