Everywhere, bagpipes, dancing and green body paint helped celebrate.
庆祝活动丰富多彩,如演奏风笛、跳踢踏舞、绿色身体彩绘等。
The green body was formed by slurry spray method on the Q235 steel substrate.
用料浆喷涂法在Q235钢基体上成形覆层坯体;
With increasing solid loading, density of AGC green body increases gradually, but strength decreases gradually.
随固相体积分数的增加,水基凝胶注模法坯体密度逐渐增加,但强度逐渐降低。
A new vacuum gel-casting was applied to ceramics which could reduce the air bubbles formed during the casting in the green body.
采用一种新型的真空凝胶注模成型法,减少了在凝胶注模成型时坯体中形成的气泡。
The green body possesses uniform particle distribution, compact structure, controllable thickness, proper flexility and tensile strength.
用雾化喷涂法或涂刷法直接在钢材或工件表面上形成厚度均匀、结构致密、粘结牢固的覆层坯体。
The influence of different shaping process on the microstructure and mechanical properties of green body and sinter was studied in this paper.
本文研究了不同成型工艺对反应烧结碳化硅陶瓷材料的素坯及烧结体的显微结构、力学性能的影响。
The optimization formula of green body of building material glazed tile has been developed using gangue as main raw materials and talcum as main flux.
以煤矸石为主要原料和滑石尾矿为主要熔剂,设计和优化了生产绿色环保建筑琉璃瓦坯体配方。
The composite green body is characterized by sufficient strength for demoulding, high density homogeneity, appropriate porosity and little dimensional change rate.
坯体具有足够的脱模强度、较高的密度均匀性和合适的孔隙率以及尺寸变化率小等特点。
Yunnan ceramic color underglaze, glaze is used directly in the dried green body has been formed on artistic creation, and then into a firing kiln at high temperature type.
云南釉下彩陶艺,是用色釉直接在已成型晾干的素坯上进行艺术创作,然后入窑经高温一次烧成型。
The present work was to determine the optimum sintering system and properties of the nanometer tetragonal polycrystalline zirconia green body by the aqueous gel tape casting process.
采用水基凝胶流延工艺制备四方多晶氧化锆薄膜,确定合理的烧成制度,并考察薄膜的显微结构与烧结性能。
For the green body containing a certain size of SiC powders, the carbon particle should be less than a certain size, or else, the density and fracture strength of RBSC decrease wit...
对于一定粒度的碳化硅粉而言,加入到生坯中碳粉粒度应小于一定尺寸,否则,陶瓷的断裂强度和密度将随碳粉粒度的增大而降低。
The effects of carbon content, moulding pressure, and carbon particle size of green body on microstructure and properties of reaction-bonded silicon carbide (RBSC) have been investigated.
研究了反应烧结碳化硅陶瓷的显微组织和性能与生坯碳含量、成型压力以及碳粉粒度的关系。
The ceramic green body is characterized by little dimensional change rate, high green body density, high homogeneity, sufficient strength for demoulding and good green body surface quality.
陶瓷坯体具有尺寸变化率小,密度较高且均匀,足够的脱模强度,表面质量好等特点。
By simulated test, the co-relationship among the slip granulometric composition, slurry deflocculation curve, mid-high pressure casting forming speed and green body shaping endurance is studied.
通过模拟试验,研究了泥浆的颗粒组成与泥浆的解胶曲线、高中压注浆成形速率及坯体挺形性等的关系。
With the increase of solids loading, the particle density increases and the bending strength of green body decreases for the network polymer accounting for only a small amount of the composition.
随着固相体积分数的增加,单位面积的颗粒分布密度增大,网络高分子在成分中只占少量,坯体抗弯强度降低。
With the increase of solids loading, the particle density increases and the bending strength of green body decreases for the network polymer accounting for only a small amount of the composition.
随着固相体积分数的增加,单位面积的颗粒分布密度增大,网络高分子在成分中只占少量,坯体抗弯强度降低。