• Experiment manifests that the leaching rates of zinc dross are elaborately enhanced and the leaching time of zinc oxide finished ore is shortened by means of ultrasonic strengthening.

    试验表明利用超声波强化浸出锌浮渣可大大提高了锌浮渣的浸出率,缩短了浸出时间。