• Using NaSCN as solvent, flat acrylic fiber was produced by two-step wet spinning process. The selection of spinneret shape and the optimization of process conditions were discussed.

    采用硫氰酸钠溶剂湿法二步法工艺生产扁平腈纶,探讨了丝板选型生产工艺优化