LDPE (Low Density Polyethylene) : Offers such advantage as tear strength and high chemical resistance. It is also waterproof.
(低密度聚乙烯):具有以下优良性质:高撕裂强度,高耐化学性,防水性。
It has a better flex cracking resistance than those of natural rubber but a lower tear strength and a higher dynamic modulus.
它比天然橡胶具有较好的抗挠曲开裂性能,但撕裂强度较低,动态模量较高。
LDPE (Low Density Polyethylene) : Offers such advantage as tear strength and high chemical resistance. It is also waterproof.
LDPE(低密度聚乙烯):具有以下优良性质:高撕裂强度,高耐化学性,防水性。
The results indicate that the X70 pipeline steel with acicular ferrite microstructure has high strength, high toughness, low transition temperature and high dynamic tear-resistance.
结果表明,本钢X70管线钢具有高强度、高抗动态撕裂能力、高低温冲击韧性以及低韧脆转变温度。
It is mainly used as rubber reinforcement and filler, to improve their elongation, tear strength and resistance to abrasion.
主要用作橡胶制品的补强剂和填充剂,能明显改善橡胶制品的抗拉强度、抗撕裂性和耐磨性。
Compared to tear resistance and tensile strength, fracture toughness is more dependent on fiber length.
断裂韧性对纤维长度的依赖性比撕裂和抗张强度大。
The influence of the loading level of nylon and PET short fibres was studied on the physical properties of Nylon-NR and PET-CR Composites, such as 20% modulus, tensile strength and tear resistance.
详细研究了尼龙和聚酯短纤维用量对尼龙-天然橡胶和聚酯-氯丁橡胶复合材料的20%定伸应力、拉伸强度及撕裂性能的影响。
The silicon and fluorine rubber with high temperature resistance, low compression permanent deformation, and high tear strength properties can meet the water sealing gasket requirements.
采用耐高温、低压缩永久变形、高抗撕裂硅、氟橡胶可以满足该部位需耐高温、耐冷却水的要求。
The properties of tensile strength, tear resistance and peeling resistance of GF/PVC tenting flexible composites are studied.
文章对GF/PVC篷盖类柔性复合材料的拉伸、撕裂和剥离的特性进行了初步研究。
The results showed that the hardness, tensile strength and tear resistance of PU increased with the increasing percentage of free NCO.
结果表明:PU弹性体的硬度、拉伸强度和撕裂强度随nco基含量增加而提高。
The results show that the presence of carbon fiber obviously enhances the hardness, heat resistance and oil resistance of the composite, but decreases the tear strength of the composite.
结果表明:炭纤维的加入能提高橡胶的硬度、耐热性及耐油性,但橡胶的扯断强度有所下降。
It has a very high tear strength, high abrasion resistance and is extremely resistant to oils and greases.
它有着高撕扯性,高耐磨性,及非常好的抗油性。
PVA modification enhances mechanical performance of NWF, tensile strength and tear resistance are increased by 25.0% and 21.6% respectively.
PVA改性增强了无纺布的力学性能,拉伸强度和撕裂强度分别提高了25.0%和21.6%。
The results showed that NBR/PVC blends exhibited good oil-resistance, ozone-resistance, and their breaking strength and tear-resistance strength were also rather improved.
结果表明,NBR/PVC共混硫化胶具有突出的耐油、耐臭氧老化性能,拉伸强度、定伸强渡和撕裂强度也较NBR有所提高。
Products with high mechanical strength, hardness large, resistant to wear and tear, withstand high temperatures, chemical resistance. corrosive characteristics of the good.
本公司产品具有机械强度高、硬度大、耐高温、耐磨损、防腐蚀、绝缘性能好等特点。
Products with high mechanical strength, hardness large, resistant to wear and tear, withstand high temperatures, chemical resistance. corrosive characteristics of the good.
本公司产品具有机械强度高、硬度大、耐高温、耐磨损、防腐蚀、绝缘性能好等特点。