The influence of additive has been analyzed by sinter pot experiment.
通过烧结杯试验,从微观和宏观上对添加剂的影响进行了分析。
The laboratory test of Hainan iron ore as bedding material was conducted in the sinter pot.
在实验室进行了海南铁矿作铺底料的烧结杯试验。
The laboratory test of Hainan iron ore as bedding material was conducted in the sinter pot.
为解决不加铺底料烧结的弊端 ,研究了用褐铁矿作烧结铺底料。
The comparative analysis between the new technology and traditional flux addition and sinter pot experiments were carried out.
在此基础上与传统熔剂的添加工艺进行了比较分析并进行了烧结杯试验研究。
This paper studied the sinter pot test of adding Robe River Ore to Ji - dong Concentrate under the sintering-operating condition of Tangshan Iron and Steel Company.
本文按唐山钢铁公司烧结工艺条件,对冀东矿配加罗伯河矿进行了烧结杯试验研究。
This article studies the influence of iron materials, basicity, fuel consumption and moisture on sinter strength through the sintering pot test and the tumbling test.
本文通过烧结杯试验和转鼓指数测定研究了铁料、碱度、燃耗和水分对水钢烧结矿强度的影响。
With sintering pot test it is found out the reasonable chemical component in sinter under the condition of Xuan Steel as well as the control range of various components for low-silicon sinter.
通过烧结杯试验,找出了宣钢原料条件下烧结矿合理化学成分、烧结矿低硅条件下各种化学成分的控制范围。
Based on pot tests with different carbon profile in sinter-bed, it is found that suitable degree of carbon segregation in three-layer is 0.4%.
通过不同燃料偏析程度的烧结杯试验,说明酒钢酸性球团烧结工艺在上中下三层的合理燃料偏析程度是0.4%。
Based on pot tests with different carbon profile in sinter-bed, it is found that suitable degree of carbon segregation in three-layer is 0.4%.
通过不同燃料偏析程度的烧结杯试验,说明酒钢酸性球团烧结工艺在上中下三层的合理燃料偏析程度是0.4%。