• When the B content is 0.05%, the coarse dendrite is found in cast structure of alloy, When B content is up to 0.1%, dendrites grow further and secondary dendrites appear.

    实验结果表明,合金组织随着B加入增加变得粗大B加入量0.05%出现粗大晶,0.1%时枝晶进一步长大且出现二次枝晶。

    youdao

  • When the B content is 0.05%, the coarse dendrite is found in cast structure of alloy, When B content is up to 0.1%, dendrites grow further and secondary dendrites appear.

    实验结果表明,合金组织随着B加入增加变得粗大B加入量0.05%出现粗大晶,0.1%时枝晶进一步长大且出现二次枝晶。