Using supercritical water oxidation process to treat RDX wastewater, the influences of reaction temperature, time and pressure on the treatment effect were discussed.
用超临界水氧化法处理黑索今(rdx)废水进行了试验研究,探讨了反应温度、时间和压力等因素对处理效果的影响。
Study on selective-oxidation kinetics and effect of oxygen partial pressure on oxidation process was conducted.
研究了选择性氧化过程动力学及氧分压对氧化过程的影响。
The effects of ultra-high pressure treatment on color, texture, oxidation of lipid, freezing and thawing process of meats were introduced in this paper.
介绍了以超高压处理时,超高压对肉的颜色、肉的组织结构、肉中脂肪的氧化、肉的冻结过程和解冻过程的影响。
This article introduced the effects of ultra high pressure on color, texture, oxidation of lipid, freezing process and thawing process of meat when meat was treated by ultra high pressure.
本文介绍了以超高压处理时,超高压对肉的颜色、肉的组织结构、肉中脂肪的氧化、肉的冻结过程和解冻过程的影响。
An improved oxidation ditch process using forced air supply low-pressure jet aeration system was used to treat middle-stage wastewater from pulping and papermaking.
采用供气式低压射流曝气系统改良型氧化沟工艺处理制浆造纸中段废水,对整个调试运行过程进行了介绍。
Taking copper sulphide mineral as study objects, the studies of chalcopyrite heating and pressure pre-oxidation leaching process were conducted in acid system adding chloride.
以硫化铜矿物为研究对象,在添加氯盐的酸性体系中,开展了黄铜矿加温、加压预氧化浸出过程研究。
The pressure biological contact oxidation process (PBCO) can effectively increase the pollutant removal efficiency by simple pressurized way.
加压生物接触氧化法通过简单的“加压”方式有效提高了污染物去除率。
This paper puts forward a new biological oxidation process to improve the ability of filling oxygen-the biological oxidation process increasing in pressure.
本文提出了一种新的改善充氧能力的生物氧化法——加压生物氧化法。
With acid hot-pressure oxidation pretreatment, the gold recovery rate of a certain refractory gold concentrate is raised from 35.6% to 94.3%, comparing to the ordinary leaching process.
采用酸性热压氧化工艺对某难处理金精矿进行预处理,其金回收率可由常规浸出的35.6%提高到94.3%。
With acid hot-pressure oxidation pretreatment, the gold recovery rate of a certain refractory gold concentrate is raised from 35.6% to 94.3%, comparing to the ordinary leaching process.
采用酸性热压氧化工艺对某难处理金精矿进行预处理,其金回收率可由常规浸出的35.6%提高到94.3%。