One stage grinding (60%-200mesh) and staged preferential flotation flowsheet is recommended for the grinding flotation scheme through the comprehensive technical and economical comparison.
对磨矿-浮选工艺流程方案,通过综合技术经济比较,推荐一段磨矿( - 2 0 0目占60 % )、分步优先浮选流程。
One stage grinding (60%-200mesh) and staged preferential flotation flowsheet is recommended for the grinding flotation scheme through the comprehensive technical and economical comparison.
对磨矿-浮选工艺流程方案,通过综合技术经济比较,推荐一段磨矿( - 2 0 0目占60 % )、分步优先浮选流程。