Properties of modified phenol resin, precoated sand preparation and property test have been narrated.
叙述了改性酚醛树脂的性能、及膜砂制备配方及其性能测定。
Precoated sand made of mixing this kind of resin and sand can serve as laser sintering material which suits laser rapid molding process much more.
这种烧结剂是一种改性酚醛树脂,它和作为耐火骨料的原砂混合制成覆膜砂作为激光烧结材料更加适用于激光快速成型过程。
Resin sand mould was adopted with precoated sand core. The upper and bottom half boxes used horizontal pouring design with box middle line as parting face.
采用树脂砂砂型、覆膜砂砂芯,上、下两个箱体均采用平做平浇的工艺方案,并选取箱体中线为分型面。
The thermal expansion values of the precoated non silica and have been measured and contrasted with them of the precoated silica sand on the same conditions.
测定了覆膜种砂在激热条件下的膨胀值,并与相同条件下普通覆膜硅砂的膨胀值进行了对比。
The thermal expansion values of the precoated non silica and have been measured and contrasted with them of the precoated silica sand on the same conditions.
测定了覆膜种砂在激热条件下的膨胀值,并与相同条件下普通覆膜硅砂的膨胀值进行了对比。