• With the further increase of DMSO concentration and reaction temperature, and the prolongation of reaction time, the molecular weight and yield of PMTFPS were decreased.

    进一步增加促进剂浓度、提高反应温度及延长反应时间,PMTFPS的分子量和产率不断下降。

    youdao

  • Poly(methyl(trifluoropropyl) siloxane)(PMTFPS) was prepared by bulk ring-opening polymerization of 1,3,5-trimethyl-trifluoropropyl cyclotrisiloxane, and crosslinked by peroxide compound.

    由1,3,5-三(甲基三氟丙基)环三硅氧烷的阴离子本体开环缩聚合成了氟硅生胶,并对生胶进行过氧化物交联。

    youdao

  • Poly(methyl(trifluoropropyl) siloxane)(PMTFPS) was prepared by bulk ring-opening polymerization of 1,3,5-trimethyl-trifluoropropyl cyclotrisiloxane, and crosslinked by peroxide compound.

    由1,3,5-三(甲基三氟丙基)环三硅氧烷的阴离子本体开环缩聚合成了氟硅生胶,并对生胶进行过氧化物交联。