• Testing for a passive surface is usually accomplished by looking for traces of free iron on the metal surface.

    钝化表面检测通常通过查看金属表面游离踪迹来完成的。

    youdao

  • The presence of exogenous surface contamination, including dirt, grease, free iron from contact with steel tooling, and so forth, may interfere with the formation of the passive film.

    外生表面污染,包括:尘土油脂来自钢铁加工游离等等可以影响到钝化生成

    youdao