A novel structure with a double step buried oxide SOI (D-SBOSOI) is developed on the basis of single step buried oxide structure.
在单面阶梯埋氧型soi结构的基础上,提出了一种双面阶梯埋氧soi新结构。
However, during hot rolling, cooling and annealing process, a complex oxide structure layer will form on the surface of stainless steel due to oxidation.
但在热轧、冷却及退火等过程中,不锈钢工件的表面因氧化会产生一层结构比较复杂的氧化皮。
Single Chamber Solid Oxide Fuel Cells (SCSOFC) has become one of the most attractive thesises for its unique properties of compact structure, simple fabrication and non-catalyst poison.
单室固体氧化物(SCSOFC)燃料电池因其结构紧凑、制造简单、催化剂不易中毒等优点,日渐成为研究的热点之一。
The influences of powder particle diameter and processing conditions upon the factors like product property, inner structure and existence of oxide in rotational molding processing were discussed.
本文讨论了摇摆滚塑成型中粉料粒径大小、工艺条件等对产品性能、内部结构、氧化物的存在及诸因素的影响。
CO2 is part of the structure of copper oxide material which should be effective.
CO2是这个结构的一部分和加有氧化铜的材料会很有效。
The electron conduction mechanism of semiconducting ceramic oxide with perovskite structure was also explained further.
对钙钛矿结构氧化物半导体陶瓷中的电子导电机制,也作了进一步的阐明。
The results showed that the passive films possessed duplex structure consisting of an outer hydroxide and an inner oxide.
实验表明,表面钝化膜形成外层为氢氧化物和内层为氧化物的双层结构。
Tenorite is an oxide of cupper which has been studied in detail on its structure, force constants and spectrum.
黑铜矿为铜的氧化矿物,对其结构、力场、光谱前人做过较详细的工作。
The results show that the film, greatly different from conventional oxide films in composition, morphology and structure, is a novel aluminum oxide film.
结果表明,该膜层的成分、形貌及结构与常规氧化膜有很大的区别,是一种新型铝氧化膜。
Some viewpoints on the forming and growing of the inactive layer and the influence of the inactive layer structure on the oxide process are given out in the paper.
并对钝化层的形成和生长,以及钝化层结构对氧化过程的影响等问题提出了自己的看法。
The significant effect of various physicochemical factors, especially the structure characteristics and cementation of free ferric oxide on the mechanical properties is reviewed.
讨论了物理化学因素,特别是结构特征和游离氧化铁的胶结作用,对力学性质的重大影响。
Chromium oxide green with corundum crystal structure has such characteristics as high thermal stability, high painted capacity, chemical corrosion-resisting capacity, etc.
刚玉晶体结构型氧化铬有高的着色力、高热稳定性及耐化学腐蚀等特点。
A gate structure of the metal oxide semiconductor is etched (510).
将金属氧化物半导体的栅极构造蚀刻(510)。
Trace water in the initiator system is an important factor which affects the initiating terminal group structure and the performance of the random copolymer of ethylene oxide and propylene oxide.
引发体系中的微量水分是影响环氧乙烷环氧丙烷无规聚醚起始端基结构,并进一步影响其分子量和使用性能的重要因素。
Its chemical structure has been determined as the zinc salt of 2-mercaptopyridine N-oxide by means of synthesizing by five steps starting with 2-aminopyridine.
为确证其化学结构,以2-氨基吡啶为原料,通过五步合成了2-巯基吡啶-N-氧化物锌盐。
For gate oxide breakdown OTP memory, we present a viable NOR array structure and current sense amplifiers.
针对栅氧化层击穿otp存储单元提出了可行的阵列结构和电流敏感放大器。
The quality of SOI wafer mainly depends on the structure of Top-Si as well as BOX (Buried Oxide).
SOI材料的质量很大程度上取决于顶层硅及埋层的结构。
Arc sprayed composite coatings are composed of iron-chromium compounds, iron oxide, and aluminum oxide with layered structure.
电弧喷涂复合涂层为典型的层状结构,主要由铁铬化合物、铁的氧化物、氧化铝组成。
A high density recording medium with a super-resolution near-field structure including a mask layer comprising high melting point metal oxide or silicon oxide is provided.
提供一种包括包含高熔点金属氧化物或氧化硅的掩蔽层的具有超分辨率近场结构的高密度记录介质。
The results show that oxide inclusion in grain boundary and structure defects from casting and forging process are the main reasons for failure of the copper sleeve.
结果表明:晶界氧化夹杂和铸造、锻造造成的组织缺陷是引起结晶器铜套快速失效的主要原因。
It was found that calcination conditions have remarkable effects on the structure and activity of the catalysts and different metal oxide supports have different optimum calcination temperatures.
实验结果表明,焙烧温度和时间对催化剂的结构和活性的影响显著,不同的金属氧化物负载的金催化剂具有不同的最佳焙烧温度。
The thermoelectric material generates by residual heat of solid oxide fuel battery, the structure is simple, the cost is low and the heat utilization efficiency is high.
热电材料利用固体氧化物燃料电池的余热发电,结构简单、成本低、热利用率高。
Rare oxide as carrier, although had obtained the structure of similar terpene compound, the yield of the myrcene obtained was in poor yield;
稀土氧化物作载体,虽有同类萜烯化合物的结构获得,但产率较低;
It seems that the amorphous iron oxide may be used as an indirect index for the evaluation of high yield paddy soils with good structure.
看来,无定形氧化铁的含量可以作为高产水稻土具有良好结构性的一个间接指标。
The relationship between cationic structure of amine and the flotation performance of zinc oxide has been discussed.
探讨了伯胺阳离子分子结构与氧化锌浮选性能的关系。
Therefore, it is very important to investigate anodic aluminum oxide films. In this paper the structure and preparation methods of porous aluminum oxide templates as well as the synthesis an...
阳极氧化铝膜具有独特的多孔结构,可作为制备各种纳米功能材料的模板,因而在纳米功能材料制备中占有重要地位。
Further study on the structure of the lignin oxide could provide a new way to modify the electrochemical property...
通过对木质素氧化产物结构的进一步研究,可为木质素的电化学改性提供了新的方法。
Described are the main usage, technical parameters, structure and application of the tank car for dense phase conveyed aluminum oxide powder.
介绍了浓相输送氧化铝粉罐车的主要用途、技术参数、结构及应用情况。
The effect of process parameters on the chemical composition and structure of titanium oxide films were studied.
研究了工艺参数对氧化钛薄膜的结构及成分的影响。
The structure and chemical compositions of the surface oxide film were investigated by XRD and Auger electron spectrometry (AES).
利用X射线衍射(XRD)和俄歇电子衍射(AES)观察了表面膜的化学成分及结构。
应用推荐