On the non preheating cladding layer, the eutectic austenite dendrite growth is along the opposite direction of temperature gradient beginning from interface to face of cladding layer.
在未预热的熔覆层内,先共晶的奥氏体枝晶的生长,从界面开始逆温度梯度方向定向生长.直到熔覆层的表面。
On the non preheating cladding layer, the eutectic austenite dendrite growth is along the opposite direction of temperature gradient beginning from interface to face of cladding layer.
在未预热的熔覆层内,先共晶的奥氏体枝晶的生长,从界面开始逆温度梯度方向定向生长.直到熔覆层的表面。