However, the creep fracture of medium strength match joint, located in the low strength base metal remote from the weld interface, showed a ductile fracture character.
中强匹配接头蠕变断裂位置在远离焊缝界面的低强度母材区,呈延性断裂性质。
The results indicate that the initial deviations of the joint positions match normal probability density function limited in the range of double mean variance.
随机缺陷分析方法中假定结构每个节点的位置偏差符合二倍均方差范围内的正态概率密度函数是可以接受的。
The results indicate that the initial deviations of the joint positions match normal probability density function limited in the range of double mean variance.
随机缺陷分析方法中假定结构每个节点的位置偏差符合二倍均方差范围内的正态概率密度函数是可以接受的。