• Based on the above straight lines, the contact zone can be determined from the known indentor curvature and loading.

    根据这些直线族,可以已知的压头曲率外载荷确定接触尺寸。

    youdao

  • The fracture toughness KIC of TiAlN coating has been measured by Weishi indenter indentor and the appearance of impress has also been observed by SEM.

    并采用维氏测量断裂韧性KIC通过扫描电子显微镜观察压痕形貌来评定涂层韧性。

    youdao

  • The fracture toughness KIC of TiAlN coating has been measured by Weishi indenter indentor and the appearance of impress has also been observed by SEM.

    并采用维氏测量断裂韧性KIC通过扫描电子显微镜观察压痕形貌来评定涂层韧性。

    youdao