Proper decrease in pouring temperature and increase in shell mold temperature are helpful to preventing hot tear.
为避免产生热裂应适当降低浇注温度,提高型壳温度。
Experimental results show that the chemical composition of molten steel has the decisive effect, whereas inclusions and pouring temperature also has remarkable influence on hot tear formation.
结果表明,在众多的影响因素中,钢水的化学成分对热裂的形成有决定性作用,而夹杂物和浇注温度对热裂的形成也有明显的影响。
BPA can leach from polycarbonate plastic bottles when it comes into contact with hot liquids and from regular wear and tear.
当聚碳酸酯塑料水壶接触到热的液体和有正常的磨损的时候,其中的BPA就会渗出来。
The two sealing machine hot and cold, stable, easy to tear cut incision can be divided into even, set variable speed, photoelectric tracking functions into one, easy to operate.
本机采用冷热两道封口,性能稳定,分切易撕切口、可分可连、集无级调速、光电跟踪等功能于一体,操作方便。
The two sealing machine hot and cold, stable, easy to tear cut incision can be divided into even, set variable speed, photoelectric tracking functions into one, easy to operate.
本机采用冷热两道封口,性能稳定,分切易撕切口、可分可连、集无级调速、光电跟踪等功能于一体,操作方便。
应用推荐