The diabase gravel almost was laminated cleavage, so the quality of aggregate by impurities and crushing was bad, segregation and bleeding of concrete made by the aggregate was heavy.
辉绿岩多为层状解理,决定了轧制或破碎的碎石骨料的质量较差,配制的混凝土离析和泌水严重;
The diabase gravel almost was laminated cleavage, so the quality of aggregate by impurities and crushing was bad, segregation and bleeding of concrete made by the aggregate was heavy.
辉绿岩多为层状解理,决定了轧制或破碎的碎石骨料的质量较差,配制的混凝土离析和泌水严重;