• A new view of characteristic zone of fusion welding joint is put forward through observations and researches of many fusion welding joints.

    通过大量熔化焊接试样观察研究,提出了熔化焊接头特征区域划分方案。

    youdao

  • The weld defects of incomplete fusion and burn through always occur when the electro-slag welding is used between the outside thin metal plate and the inner clapboard in a box-section member.

    箱形截面构件薄壁隔板焊接,易产生壁板穿焊缝未熔合现象。

    youdao

  • A new view of characteristic zone of fusion welding joint is put forward through observations and researches of many fusion welding joints.

    本文研究了已提出几种熔焊接头特征区域划分方案,找出认识一致认识分歧之处,并认识分歧的原因进行了详细讨论。

    youdao

  • A new view of characteristic zone of fusion welding joint is put forward through observations and researches of many fusion welding joints.

    本文研究了已提出几种熔焊接头特征区域划分方案,找出认识一致认识分歧之处,并认识分歧的原因进行了详细讨论。