In this paper, the critical exposure (Ec) and the penetration depth (Dp) of the myself prepared photosensitive resin were determined, and its critical exposure is 8.
本文对自制备的光敏树脂的临界曝光量和透射深度这两个特性参数进行了测试研究,测得临界曝光量为8。
In this paper, the critical exposure (Ec) and the penetration depth (Dp) of the myself prepared photosensitive resin were determined, and its critical exposure is 8.
本文对自制备的光敏树脂的临界曝光量和透射深度这两个特性参数进行了测试研究,测得临界曝光量为8。